Thursday, October 4, 2012

Re: [MW:15466] Interpretation of Clause QW 407.2 of ASME SEC. IX

Yes you can use . But you have to specify the temp range (for ur job) on wps

M.Sakthi mugunthan

On Oct 2, 2012 8:21 PM, "shah satish" <shahsatish34@gmail.com> wrote:
Dear All,
Hi,
I have a one PQR with PWHT,Heat treatment cycle is 660 - 665 Deg. C
Temp. and time 95 minutes, and my job  Heat treatment cycle 660 - 665
Deg. C. Temp and soking time 40 minutes (min).can i use this pqr for
job.

Thanks

Satish,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...