Wednesday, October 3, 2012

Re: [MW:15458] Wire type IQI

IQI just certified your image is OK or not, the importance is size of the visible wires on the certified Radiographic Film, so your responsibility is identified a deviation of size of ISO IQI wires and ATSM IQI wires, if it's same then OK.

P.S: What's specification of ISO IQI?

CMQ

Ngày 01-10-2012, vào lúc 07:13 CH, <pankaj.kolhe@wipro.com> viết:

<image001.gif>

Dear sir,

Is it permissible to use ISO  type wire IQI instead of ASTM type?, please give me the code reference

If yes then how to decide, which wire is required to be visible in ISO type wire IQI?

 

Regards

Pankaj Kolhe

QC Dept.

Wipro Limited (Wipro Water)  

Serene Properties Private Limited, SEZ, Plot No. 3, Building No. 7, 6th Floor, TTC Industrial Area, Thane-Belapur Road, Airoli, Navi Mumbai – 400708, Maharashtra, India.  Tel- +91 22 39302135   E-mail- pankaj.kolhe@wipro.com 

 

Please do not print this email unless it is absolutely necessary.

The information contained in this electronic message and any attachments to this message are intended for the exclusive use of the addressee(s) and may contain proprietary, confidential or privileged information. If you are not the intended recipient, you should not disseminate, distribute or copy this e-mail. Please notify the sender immediately and destroy all copies of this message and any attachments.

WARNING: Computer viruses can be transmitted via email. The recipient should check this email and any attachments for the presence of viruses. The company accepts no liability for any damage caused by any virus transmitted by this email.

www.wipro.com

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...