Dear Prashant I do not understand why are yoy complicating the PQR with CS backing For your purpose you can qualify PQR i) Monel to Monel of Butt weld ii) Monel to CS butt above PQR will help you to weld Butt and Fillet Regards Hegde P.B.
--- On Tue, 2/10/12, prashant pansare <prashant.pan17@gmail.com> wrote:
From: prashant pansare <prashant.pan17@gmail.com> Subject: [MW:15448] Welding Procedure - Monel to Monel To: "mat wel" <materials-welding@googlegroups.com> Date: Tuesday, 2 October, 2012, 6:39 PM
Dear All,
I am qualifying Welding Procedure - Monel to Monel butt weld with CS backing. On basis of the same can I qualify Welding Procedure for Monel to CS in fillet position?
Regds, Prashant Pansare (IRS - Mumbai)
-- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/ http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment