Re: [MW:15457] A 333 Gr 6 to use for low temperature

Dear All,

Main Chemical Contain is Carbon and Magenis ratio is required. is perticulur given standard ratio.

Kaushik PAtel


On Wed, Oct 3, 2012 at 9:23 AM, kishor kaku <kkaku067@gmail.com> wrote:
Manganese!


On Tue, Oct 2, 2012 at 6:35 PM, prashant pansare <prashant.pan17@gmail.com> wrote:
Dear All, 

Which element makes A 333 Gr 6 to use for low temperature condition.

Regds, 

--
Prashant  Pansare
(IRS - Mumbai)


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 



--
Thanks & Regard's


Kaushik Patel,
Surveyor,
Bureau Veritas - Gandhidham
63, Shivdhara Nagar,
Plot No. 163, Nr. Purshottam nagar,
Adipur - Gandhidham.
Mobile: +91 9687000073, 9427599638.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...