Dear forum members,
Kindly be sharing my concerns about "deeply rusted materials " (different sizes, thickness about 9.53mm). the appearance of the
materials are poor. the thickness is measured by UT gauge and found in required limits. but the mill coating of materials are damaged
in most of the cases, which is the main issue...are these are really to be rejected in client point of view ( elbows- WPB-234, A 106 pipes etc...)...these materials were stored in poor conditions with supplier... expecting opinions fromm all corners...
NB: photos attached.
regards,
Kumar.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.