I want ur opinion on following matters
WPS qualification of Piping higher thickenss above 19mm (Dia 12" to 36") welding with two welders.==SEC IX
Question-1: Is it require one welder should weld entire circumference(ROOT+HOT) ;then second welder weld entire circumference (FILL+CAP)
YES OR NO
Question-2 Both the welder weld half circumference at same time (side-A 12-9-6,,,,SIde-B 12-3-6)===SEC IX
YES OR NO.
Question 3 : OR its depend on WPS how we have qualified with welder situation.(as per Question-1&Question-2)
YES OR NO.
regards,
mohd.
-- To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment