Dear Samshuddin,
1. Attached Sketch might usefull for better understanding ( ignore the PG-PDS additional client requirement)
2. It's not each process (refer sketch)
3. Even you can go for 3cycle PWHT.
 
Regards,
Kavin Murugam
0126159644
 

From: samshuddin k <sam.renja@gmail.com>
To: materials-welding <materials-welding@googlegroups.com>
Sent: Sunday, March 18, 2012 10:59 PM
Subject: [MW:13920] Impact test requirements as per UG 84

Dear Experts
I have to prepare a PQR for SA 516 Gr.70 plate of 50mm thick.
I am using GTAW+SMAW+SAW(10mm+20mm+20mm)
My doubt is how many test specimen i have take for impact test
Is that i have to take HAZ & WELD from each process.
Please expalin.
And as per UCS 56, I am going to do PWHT.
Then can i take twice the holding time to considering the on job repair.
Is that acceptable
Please advise
Samshuddin.K
Asst QA Engineer
NKOM QATAR

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...