[MW:13965] WELDING OF SA 240 310S

 

Hi all,

We facing problem to weld SA240 310S material. We found linier indication(crack) in Radiography testing.

Once the repair comes then after repair we found more liner indication.

 

Thanks & Regards,

Mukesh Chaudhari