Tuesday, January 10, 2012

Re: [MW:13449] NDE FOR BUTT WELD

I would not suggest to bend the film cassette. UT using angle and straight probes is more appropriate. However I am surprised that there is no a tapered transition as required by most of the codes in case of unequal thickness
Best regards
Dr Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
HBS Regional Technical Manager


  From: "Desai Jignesh (Mumbai - Piping)" [J.J.Desai@ticb.com]
  Sent: 10/01/2012 15:27 ZE5B
  To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
  Subject: [MW:13441] NDE FOR BUTT WELD


Can somebody write me about the possibility of either radiography OR Ultrasonic testing of attached butt weld?

 

We have tried to carry out radiography with and without non metallic support as in the attached snaps but image is not clear.

 

Regds/Jignesh


No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...