Dear All,

As per Sec IX 2011 a , there were some changes in Heat input
calculation regarding overlay. Can any body explain me with expample.

We have one corrosion overlay qualified on CS material with E309LMO and E 316L.

The heat input for first pass is 0.815 KJ/mm
, second pass 0.7 KJ /mm
final pass 0.715 KJ/mm

What changes to done in in the WPS as per ASME Sex. 2011a.


Regards

Venkat

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...