Hi

 

There is some specific requirements for Straight Flange in formed dish heads with respect to the

 

-       Thickness difference between shell and dish head (Thickness diff by more than 3mm or 1/4th of thinner whichever is less, requires 1:3 transition, Ref UW-9 (c) and UW-13(b)(2)).

-       Type of attachment(Fig UW 13.1)

-       Side to pressure (UG-32 and UG-33)

 

Refer the following clauses UG-32 (l),(m), (n) and UG-33(i), and UW-13 for further details.

BR

M.Vijayan

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of kcrtechnical
Sent: Thursday, January 05, 2012 11:38 AM
To: materials-welding@googlegroups.com
Subject: [MW:13413] Straight Face Requirement in Dished End..Reg.,

 

Dear Friends,

 

Is there any specific requirement specified any PV Codes regarding requirement of Straight Face in Dished Ends.

 

Best regards

K C R

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



This communication and any files transmitted with it are confidential and may also be privileged. It is for the exclusive use of the intended recipient(s). If you are not the intended recipient or the person responsible for delivering it to the intended recipient(s), please note that any form of distribution, copying or use of this communication or information contained in it is strictly prohibited and may be unlawful. If you have received this communication in error please return it to the sender, and delete the material from any computer. We reserve the right to monitor email communications through normal internal and external networks. We believe but not warrant that the email and the attachments are virus free. The statement and opinions expressed in this communication are those of the writer and do not necessarily represent those of Madina Group, whose registered office address is

P.O. Box 20459, Doha, Qatar.
Tel. +974 44600818
Fax. +974 44603143

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...