Dear MPK,
Major reason for air test is to check the water tightness, hydro test is for integrity(strength) of the structure or piping
With regards
Vimal Kumar
+65 9100 2565
Dear Experts,why phenumatic test is more critical than hydro test?Thank you,MPK--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments
air is compressible. it leads in to rupture, if the test fails, which makes the pressure vessel unrepairable whereas in liquid the most cases will end in small failure which can be repairable.
Regards
Venkatesh