Hi Babu
In one of my past Nuclear assignments,i had conducted a PQR of Pipe # Plate with full penetration. It was a class 1 component for a nuclear reactor as per ASME Sec III NB.
The PQR testing requirements were as per client specifications only i.e we had to do only UT and macro.In those specs. the joint geometry and welding position during procedure qualification was an essential variable !
Regards
Prem S Nautiyal
Mobile:+91 9004063879 / 9769316004
On Thu, 04 Aug 2011 10:33:42 +0530 wrote
>Gents,
�
Some one share info on the above subject.
�
DNV is not discuss about this kind of configuration.
Thanks & regards,
K.Babu
--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
PREM S NAUTIYAL
CELL : 9769316004
Treat yourself at a restaurant, spa, resort and much more with Rediff Deal ho jaye! --
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
No comments:
Post a Comment