Dear Ashish,

I think that you should consider the following points,analyze
according to your suitability standards and frame your own product
standard for
Welding Electrode holder.
The points are:
1. The conductivity of the contact jaw should be maintained & tested
whether u use solid formed type design or brazed type design.
2. The holding portion of the holder should have enough insulation to
protect welders from shock.The insulation should be tested.
3. The weight of the welding holder should be such that welders
shouldn't have any problem to use it in any position.
4. The spring constant of spring in holder should be considered.

by analyzing above points, frame ur own product standard and then use
it in ur way.It will be as good as ur other standards.

Regards
Sushant Thakur

On Jul 28, 8:28 am, Ash_Ish Soni <ashishson...@gmail.com> wrote:
> Dear Member,
>
> I have come across to know that our contractor is using Welding Electrode
> Holder as per the attached photo. Contractor is big enough to force without
> standard, so, I am searching for any International Standard which helps to
> force them to replace this kind of Welding Electrode Holder with the
> Standard one, which all of you know.
>
> I have come to know one standard - IEC - 60974 - 11, but that is only for
> Safety point of view, which is not enough.
>
> Request for the help.
>
> Thanks & Regards,
>
> Ashish Soni.
> Essar.
>
>  Welding Electrode Holder.docx
> 944KViewDownload

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...