Monday, April 25, 2011

Re: RE: [MW:10838] Impact testing temp. for EN19 steel

Hi Babu

Thanks for your reply.
However my second query is unadressed.

"Secondly i would also like to know which of the two will have more toughness and why - EN 19 casting OR EN19 plate ?"

I feel that plate will have more toughness than casting, but how much ???

Can anyone reply to this please ??

Regards

Prem Nautiyal




On Fri, 22 Apr 2011 21:47:03 +0530 wrote
>




















Hello !



Please can someone answer my general
query>



Why only Charpy V Notch Testing is mostly
used for Impact Testing & why Izod is not popular.



Please give detailed information to
understand process thoroughly.



Waiting for replies!





Regards,

Manmeet
Magdum

Document Quality Control – Drilling Riser Systems

QS Supply Chain.

AkerSolutions



( (Tel ) +91-20-66918751

Ë (Mobile)
+91 9762446730

* (Email) Magdum.Manmmet@akersolutions.com

Aker Powergas Subsea Pvt Ltd

BlueRidge , IT-2, Flagship Infrastructure Pvt
Ltd, Ist Floor, Hinjewadi, Pune 411045, India

Registered in India
; CIN;U74990MH2010PTC210736













From:
materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kathalingam Babu

Sent: Thursday, April 21, 2011 5:47 AM

To:
materials-welding@googlegroups.com

Subject: Re: [MW:10765] Impact
testing temp. for EN19 steel







Hi











Izod will be done at Room temp., Unless otherwise
specifically mentioned by spec.











Thanks & Regards,











K. Babu







----- Original Message -----





From: PREM
SHANKARDUTT NAUTIYAL





To: materials-welding@googlegroups.com






Sent: Wednesday, April 20, 2011 11:21 PM





Subject: [MW:10758] Impact
testing temp. for EN19 steel









Dear Friends



I wanted to use EN 19 plate in one of my present project, wherein the
application demands severe impact loads at room temperature.



I had browsed through the properties of EN 19 plate in various literatures
wherein the Izod test values are mentioned @ 55J.



However the Izod testing temperature is not mentioned.



Can anyone help me out or guide me where to refer, so that i can know the Izod
testing temperature of this EN 19 steel.



Secondly i would also like to know which of the two will have more toughness
and why - EN 19 casting OR EN19 plate ?

The reason being the final component will have to be casted due geometrical
complications.





Regards



Prem Nautiyal





PREM S NAUTIYAL

CELL : 9769316004









--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions w.r.t.
applicable code/standard/contract documents.





This e-mail and any attachment are confidential and may be privileged or otherwise protected from disclosure. It is solely intended for the person(s) named above. If you are not the intended recipient, any reading, use, disclosure, copying or distribution of all or parts of this e-mail or associated attachments is strictly prohibited. If you are not an intended recipient, please notify the sender immediately by replying to this message or by telephone and delete this e-mail and any attachments permanently from your system.





--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>



--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>


PREM S NAUTIYAL
CELL : 9769316004

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...