Tuesday, April 26, 2011

RE: [MW:10860] ASME/ASTM equivalent of S355J2+N

A516 Gr70 is ok to substitute.
 

From: kathalingam.qaqc@ppl.com.sg
To: materials-welding@googlegroups.com
Subject: Re: [MW:10856] ASME/ASTM equivalent of S355J2+N
Date: Tue, 26 Apr 2011 16:24:40 +0800

ABS Grade EH36
Also, ASTM A131 Gr.EH36
 
Thanks & Regards,
 
K. Babu
----- Original Message -----
Sent: Tuesday, April 26, 2011 4:09 PM
Subject: [MW:10855] ASME/ASTM equivalent of S355J2+N

Dear All

What is the ASTM/ASME equivalent of structural material S355J2+N (minimum yield strength 355 MPa, Tensile 470 to 630 MPa, C: 0.20 max, Si: 0.55 max, Mn: 1.60 max , CE: 0.45 max). A link to reference document stating the same would be much appreciated.

Thanks & best regards

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...