On Mon, Apr 25, 2011 at 12:29 PM, Abdul Wahab <awengineer@gmail.com> wrote:
Dear All Professionals,
I am facing a problem & i hope that i will recieve a positive feed
back from u all,
Case 1.
Pipe butt joint is coming directly over the pipe rack. Is there any
issue?
Case 2.
Pipe suppor pad / RF Psd is coming over the butt joint, Is tehre any
issue?
Please answer with reference of international standrd & what is the
best practice to get ridoff such kind of issues.
Best Regard,
Abdul Wahab
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Dear Friend
RF pad is not allowed in any case over the but joints.It is advisable to shift the pipe rack horizontal member avay from the joint.
--
--
Thanking You.
Yours faithfully
For
TOLANI Projects Pvt.Ltd.
TOLANI Projects Pvt.Ltd.
J.R.Parmar
09159991454
08000040871
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments