RE: [MW:10825] usage of 45 deg elbow cut from 90 deg elbow.

Dear Murty,
 
When we required 55 deg or 60 deg elbow, we normally cut is from 90 deg elbow. Because these are not the standard item.
You can cut 90 deg elbow to 45 provided the dimension remain same as per ASME B16.9.
 
Regards.
 

Date: Sun, 24 Apr 2011 07:27:42 -0400
Subject: Re: [MW:10824] usage of 45 deg elbow cut from 90 deg elbow.
From: jmadukayil@gmail.com
To: materials-welding@googlegroups.com


45° Elbows are available as standard items. Why cut a 90° elbow?
In case you cut a 90° elbow to 45° - the 45° elbow here becomes a non standard item.


On Sun, Apr 24, 2011 at 7:15 AM, narasimha murthy <jnm71269@gmail.com> wrote:
Dear All,
 
Please suggest if you can cut a 90 deg elbow and use as 45 Deg elbow is it acceptable practice and if so is there any code refered to such usage.
 
Regards,
 
Murthy

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...