Re: [MW:10822] ASME sect IX PQR thick Qualified

In WPS, Base Material thick will have min and max range and weld metal deposit will have max to be deposited only, in ur case Gtaw may be used to deposit from 1.5mm to Max 12mm weld deposit and SMAW may also be used to deposit from 1.5mm to max 18mm. u can use this pqr
Pandithan

On Sat, Apr 23, 2011 at 2:03 PM, Zakaria ghrab <zakaria.ghrab@gmail.com> wrote:
Hi all,

  We have a PQR, 15 mm Thickness, welded 6mm GTAW, 9mm SMAW.
According ASME sect IX, table QW-451.1, the Qualified Thickness "T" of base metal qualified will be 1.5 mm to 30 mm and the deposit weld thikness GTAW will be 12 mm max "2xt".
 Means if i have to weld pipe thick 3 mm i can't use this PQR, i'm right ?

--
زكرياء غراب


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...