Re: [MW:10804] ceramic welding

DEAR PRAKASH,
THERE ARE TWO METHODS.ACTIVE BRAZING ALLOYS FOR BRAZING AND TWO STEP BRAZING (METALLIZING,BRAZING WITH SUITABLE ALLOY.)TIG IS NOT POSSIBLE. TO MY KNOWLEDGE.
DrK G K MURTI.

On Fri, Apr 22, 2011 at 12:05 PM, gajjalla surya prakash <gajjalla@gmail.com> wrote:
dear all ,


is it possible to do tig welding of ceramic materials .



--
With regards,

Surya Prakash Gajjalla
ASSOCIATED ENGINEERING SERVICES
3-5-944/220-221 panchavatimall narayanaguda hyderabad india 500029.

www.aesinspections.com
0091 9885162668

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...