I believe you should be in AWS D1.6, for structural stainless. There
is an option for prequalificaiton in this code, which means you do not
have to make a PQR and the associated tests

On Apr 25, 5:57 am, Martin Prad <martin_p...@hotmail.com> wrote:
> Dear friends,
>
> What tests are required for generating of new WPS for 3 mm ss plate?
> Qualification code is AWS D1.1
> Available material for welding is 3 mm ss plate.
> Welding process is TIG.
>
> best regards,                                    

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...