@ Karthik sir
As per Note 5, Can I have to go for 4 side bend instead of root &
face?.
or Either of two face & root or side bend whatever we can na?
reply me.
Regards
Srinivas.
On Mar 2, 5:59 am, Karthik <karthik6...@yahoo.com> wrote:
> Hi,
> Yes You are correct.But Instead of Root and face bend test..it can be replaced by 4 Side bend test as per QW451.1 - Note.5.
>
> Thanks & Regards,
>
> (Karthik)
>
> Karthikeyan.S QA/QC Manager Getabec Energy Co.,Ltd. 379,Moo6,Soi8,Nikhomphatana, Rayong-21180, Thailand. Phone: 0066 38 897035-8 (Off) Fax: 0066 38 897034 Hand Phone: 0066 892512282
>
> --- On Tue, 3/1/11, Srinivas Engr <srinivas.gmsr...@gmail.com> wrote:
>
> From: Srinivas Engr <srinivas.gmsr...@gmail.com>
> Subject: [MW:10070] Seeking advice in Mechanical Testing of 8" SCH 80 pipe test coupon as per ASME SEC 9
> To: "Materials & Welding" <materials-welding@googlegroups.com>
> Date: Tuesday, March 1, 2011, 5:08 PM
>
> Dear All
>
> My test Coupon is 8" SCH 80 Thk 12.7mm A 106 Gr.b, ( No PWHT & NO
> toughness)
> As per asme sec9, from QW 451.1
> the mechanical test required is Tension test - 2Nos
> Face Bend - 2nos
> Root bend - 2nos.
> & I thought the above test are enough for making PQR & WPS.
> am i right?
> or else any other test is required r not?
>
> regards
> Srinivas
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg athttp://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.