Hi,
01.Diffrence:Butane is not a highly toxic gas. Therefore, it can be safely, properly stored inside with  little worry. You can also extract approximately 12 percent more energy per liter from butane than you can propane, which means that, liter for liter, you will get more mileage out of butane. Butane is also a cheaper gas to purchase, though propane is more widely available . (extract from the article)
02.For WPS - Change in the type of preheat/type of gas is not an essential variable.Some customer specifications may restrict while you do on site.So pls.refer to project spec.if you work on site.
Thanks & Regards,
 
(karthik)

Karthikeyan.S
QA/QC Manager
Getabec Energy Co.,Ltd.
379,Moo6,Soi8,Nikhomphatana,
Rayong-21180,
Thailand.
Phone: 0066 38 897035-8 (Off)
Fax: 0066 38 897034
Hand Phone: 0066 892512282


--- On Tue, 8/31/10, eduardocalva@hotmail.com <eduardocalva@hotmail.com> wrote:

From: eduardocalva@hotmail.com <eduardocalva@hotmail.com>
Subject: [MW:6794] Propane or butane to preheat
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Tuesday, August 31, 2010, 1:30 AM

Could all of you tell me the difference between preheat with propane
and butane?, If a WPS is qualified by preheating with propane but
butane is used in production welds is wrong?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...