Pls note that , 9Cr-1Mo/9Cr-1Mo-V Steels are the Ferritic Steels.
Don't confuse Sigma embitterment of ASS with Ferritic Steels.
Regards,
K.Babu
Singapore
----- Original Message ----- 
From: "Abby Joseph" <abbyjoseph@gmail.com>
To: "Materials & Welding" <materials-welding@googlegroups.com>
Sent: Monday, August 30, 2010 4:37 PM
Subject: [MW:6775] 9Cr-1Mo/9Cr-1Mo-V steel welds
> Do 9Cr-1Mo/9Cr-1Mo-V steel welds also develop sigma phase during
> service, like some stainless steels?
> (Note- these alloys also contain substantial wt% of Cr, Fe and Mo.
> They are also exposed to the high temp at which sigma phase forms.)
> If not, why?
>
> Regards,
>
> Abby Joseph
>
> -- 
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to 
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at 
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and 
> meant for educational purposes only, Users must take their own decisions 
> w.r.t. applicable code/standard/contract documents.
> 
-- 
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/