Hi

If you are referring ASME Sec IX, then as per the table of QW-253 which talks about welding variables procedure specifications, refer QW-409.4 (Electrical characteristics), change in current or polarity is considered as supplementary essential variable for Impact requirements and Non-essential if you don't have any Impact requirements.


Regards

Prem Nautiyal

On Sat, 28 Aug 2010 15:26:12 +0530 wrote
>Dear all





If one qualifies in DCEP for SMAW,

Whats the range qualified for those either DCEP only or both (DCEP&

DCEN)?

any limits given in specs? where?





Thanks



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...