Re: [MW:6757] Polarity qualification?


Hi

If you refer ASME Sec IX, QW-253 table, which talks about the welding variables procedure specifications for SMAW, then refer QW-409.4 (electrical characteristics), which mentions that a change in current or polarity is Supplementary essential variable for Impact requirements and Non-Essential variable for Non-impact requirements.
What is your case?


Regards

Prem Nautiyal

On Sat, 28 Aug 2010 15:26:12 +0530 wrote
>Dear all





If one qualifies in DCEP for SMAW,

Whats the range qualified for those either DCEP only or both (DCEP&

DCEN)?

any limits given in specs? where?





Thanks



--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



PREM S NAUTIYAL
CELL : 9820313278

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...