Re: [MW:6750] Thinning percentage of Ellipsoidal dish end.

Dear Mr. Kisan,

Better you ask to your head maker.
It is depend on making process, plate thickness and material type.

Small size of ED head can be made using forming dies, such as making CAP.
Big size and thin thickness can be finished by spinning in cold
condition, meanwhile thicker plate made in hot condition.
I used Hokkai japan to make certain size of head, they provide
"thickness after forming" in their catalog for our estimation when
design. In a formal, they will inform "guarantee thickness after
forming" in a quotation.

As a sample you can see such table from Hokkai China on
http://www.hokkai.com.cn/e22g.htm

And usually not use percentage.

Thank you.

Tex Riz


On Fri, Aug 27, 2010 at 6:55 PM, Kisan Gamane
<kisankrishna1506@gmail.com> wrote:
> Dear all
> Anybody can tell me about how many percentage thicness will be gets thin in
> ellipsoidal dish end?
>
> --
> Thanks & regards
> Kisan Gamane
>
> ॐ सर्वे भवन्तु सुखिनः, सर्वे सन्तु  निरामयः
> सर्वे  भद्राणि  पश्यन्तु, मा कश्चिद दुखभाग भवेत्.
> May all be happy. May all enjoy health and freedom from disease.
> May all have prosperity and good luck. May none suffer or fall on evil days.
> ++++
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
Regards,

T. Rizal Hidayat

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...