Hi,
Acceptance criteria for defect depend on standard,code or spec. in project such as ASME, AWS, BSI, GL, BV,... .
ASME : Undercut, LOF, LOP, Crack = 0.
AWS: Undercut in static condition=0.8 mm, dynamic condition=0. LOF and LOP=0.

--- On Thu, 8/26/10, aslam khan <aslamkhan4u@gmail.com> wrote:

From: aslam khan <aslamkhan4u@gmail.com>
Subject: [MW:6736] acceptance criteria of DPT
To: materials-welding@googlegroups.com
Date: Thursday, August 26, 2010, 10:32 AM

HI FRIENDS,
CAN ANY BODY TELL ME ABOUT THE ACCEPTANCE CRITERIA OF DPT ?ACCEPTANCE RANGES OF DEFECTS LIKE UNDERCUT,PORE,POROSITY,CRACK,etc.thanks
 
Regards
M.Aslam Khan
QA/QC ENGINEER
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...