with that pqr u have to carry out welding with existing essential variables without anychange and supplimentary essential variables. u need not do tensile and bend test, u have to do only impact test and rewrite another wps or make revision
kgp

On Thu, Aug 26, 2010 at 5:31 AM, Larry <quality@unieng.com.au> wrote:

Hi There,

 

We have an existing WPS, The existing WPS doesn't have a cold service specification, and we would like to do a test coupon from that WPS and have it charpy tested, so we can revised the existing WPS. Now the requirement of the client is -70 degrees Celsius. Is that alright or do we have to do another PQR? Code is ASME IX.

 

 

Thank you,

 

Larry Zarate

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...