Thursday, August 26, 2010

Re: [MW:6729] Impact requirements for API 5L X52 PSL2

those two codes do no have any impact test requirements just like section I and B31.1.
If you want the assess you piping for low temperature service you may use ASME B31.3 Chapter III - 323.2.2

Dr. G. Dilintas - Authorized Inspector Supervisor
I&F Regional Technical Manager
Bureau Veritas Piraeus - Greece
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Inactive hide details for Sajish <sajishjm@gmail.com>Sajish <sajishjm@gmail.com>


          Sajish <sajishjm@gmail.com>
          Sent by: materials-welding@googlegroups.com

          25/08/2010 22:39

          Please respond to
          materials-welding@googlegroups.com

To

"Materials & Welding" <materials-welding@googlegroups.com>

cc


Subject

[MW:6717] Impact requirements for API 5L X52 PSL2

Ref


Hi,

Can anyone clarify wether impact testing is required for API 5L PSL2
Code of construction is ASME B31.8
and for B31.4
Would be qualifying the procedure as per ASME Sec IX.

Thanks in advance
Sajish

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...