Re: [MW:6729] Charpy Test

You have to do an other PQR and register all supplementary essential parameters.

Dr. G. Dilintas - Authorized Inspector Supervisor
I&F Regional Technical Manager
Bureau Veritas Piraeus - Greece
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04
Inactive hide details for "Larry" <quality@unieng.com.au>"Larry" <quality@unieng.com.au>


          "Larry" <quality@unieng.com.au>
          Sent by: materials-welding@googlegroups.com

          26/08/2010 03:01

          Please respond to
          materials-welding@googlegroups.com

To

<materials-welding@googlegroups.com>

cc


Subject

[MW:6716] Charpy Test

Ref


Hi There,

We have an existing WPS, The existing WPS doesn't have a cold service specification, and we would like to do a test coupon from that WPS and have it charpy tested, so we can revised the existing WPS. Now the requirement of the client is -70 degrees Celsius. Is that alright or do we have to do another PQR? Code is ASME IX.


Thank you,

Larry Zarate

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...