Wednesday, August 25, 2010

Re: [MW:6719] Reg Range of Amperage in WPS

I'm not clear with your answer. can give me an more info

--- On Wed, 25/8/10, Muhammed Ibrahim PK <ibratech@gmail.com> wrote:

From: Muhammed Ibrahim PK <ibratech@gmail.com>
Subject: Re: [MW:6708] Reg Range of Amperage in WPS
To: materials-welding@googlegroups.com
Date: Wednesday, 25 August, 2010, 7:29 PM

Hi,
 
Control the maximum range to control heat input.

Thanks & Regards
Muhammed Ibrahim PK



On 25 August 2010 17:34, ayys4u <ayys4u@gmail.com> wrote:
Dear All,

Can any one help me!

PQR Qualified with an amperage of min 350 and max 550.
As per AWS D1.1, Allowable Variation in Amperage for WPS  is 10 %.
How should i consider this 10%.

Case 1
Should i Consider lesser 10 % lesser to  PQR's Min Amperage and
Greater side 10 % to the max PQR Amperage.

Case 2
 Or Should i consider 10% min max of Average of PQR Value.

Which case is correct?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...