[MW:6808] RE: 6805] Required Tests

For ferritic materials (carbon steel, alloy steel, stainless steel) EN 287-1, Approval testing of welders – Fusion welding – Part 1:  Steels.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Eng/ Mostafa Kamel Hussein
Sent: Tuesday, August 31, 2010 3:37 AM
To: materials-welding@googlegroups.com
Subject: [MW:6805] Required Tests

 

Dear,

I hope to the required tests need for the welder performance qualification (WPQ) according to the EN code and i hope to know the name of this code?

SaSa

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...