John du Plessis
Technology Manager
Tel: +27 (11) 298 2100
Tel: +27 (11) 298 2103 (Direct)
Fax: +27 (11) 836 6014
Mobile:+27 82 883 4970
www.saiw.co.za
This email and any files transmitted with it are confidential and may be
legally privileged. They are intended solely for the use of the individual
or entity to whom they are addressed. Access to this e-mail by anyone else
is unauthorised, and any disclosure, copying, distribution or other use of
this e-mail is prohibited and may be unlawful. We will not under any
circumstances have any responsibility or liability arising out of or in
connection with any unauthorised use of this e-mail. If you have received
this email in error please notify the sender before deleting it.
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of
eduardocalva@hotmail.com
Sent: 30 August 2010 08:31 PM
To: Materials & Welding
Subject: [MW:6794] Propane or butane to preheat
Could all of you tell me the difference between preheat with propane
and butane?, If a WPS is qualified by preheating with propane but
butane is used in production welds is wrong?
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments