Hello,

Could someone tell me please what is the best filler metal to make a
buttering over A-217 Gr WC9 base metal.

Are there special recommendations?

I will appreciate answers!

Luis Carlos

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

1 comment:

quang said...

hi Luis Carlos,
i think you can you E9016-B3 và E9015-B9.