Saturday, August 28, 2010

[MW:6753] What is SR(PWHT) thickness requirements by AWS D1.1

Dear all,

what r thickness to be done for SR(PWHT) for CS according to AWS D1.1
structural steel code?
Where to refer in AWS D1.1? for thickness requirements for PWHT?

Thanks
Srinivas

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...