RE: [MW:4396] Pullout load calculation of tube to tube sheet weld

Mr. Ibrahim

 

Please refer Non Mandatory appendix A , of ASME section viii div 1.

 

Also as per UW 20, welded joints do not call for shear load calculation .

 

Regards

 

Prashanth

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Muhammed Ibrahim
Sent: Saturday, February 27, 2010 1:56 PM
To: materials-welding@googlegroups.com
Subject: [MW:4395] Pullout load calculation of tube to tube sheet weld

 

Hi Members,

 

Anybody have the pullout test load calculation of tube to tube sheet weld with different joint design?. If any articles avilable in pdf. please send.

Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



Please don't print this e-mail unless you really need to.
*******************************************************************
This e-mail is confidential. It may also be legally privileged. If you are not the addressee you may not copy, forward, disclose or use any part of it. If you have received this message in error, please delete it and all copies from your system and notify the sender immediately by return e-mail. Internet communications cannot be guaranteed to be timely, secure, error or virus-free. The sender does not accept liability for any errors or omissions.
*******************************************************************
"SAVE PAPER - THINK BEFORE YOU PRINT!"

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...