Friday, February 26, 2010

Re: [MW:4382] Failure of PQR in All Weld Tensile

Where do you get the failure? Base or weld metal?


  From: prashant pansare [prashantpan_99@yahoo.co.in]
  Sent: 26/02/2010 12:39 ZE5B
  To: mat wel <materials-welding@googlegroups.com>
  Cc: par kat <paresh.katvi@bg-group.com>; roj abra <roji.abraham@bg-group.com>
  Subject: [MW:4381] Failure of PQR in All Weld Tensile


Dear All,
We are working on PQR & deatails are as folows :
Appl. Code - DNV OS F101,2000
PQR - Through THickness Repair. (SMAW)
Base Metal - API 5L X GRADE 60 - 12.75" OD X 14.3 mm THK.
Filler Metal - E-7018 H4R
Position -6G
After mechanical tests, we are getting all values in acceptable limits except All Weld Tensile results.(Reqd- 517 Mpa & Actual - 483 / 493 Mpa)
What is the reason & solution for the same?
Pl. reply.
PSP  


Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...