Friday, February 19, 2010

Re: [MW:4344] paintwork marks adjacent to weld joints, welding flux, stain mark during the CCTV inspection for new O2 piping

Dear
                We have seen your Detail mail regardig the O2 line cleaning. Here in our project we had a same issue construction team erected 20 spools SS 10 IN DIAwith out internal cleanig........after long discussion we cut outall the joints they did chemical cleanig after cleaning we gone for UV LAMP inspection.
Regards
Mano

2010/2/19 Vinod Jotwani <poojvin@yahoo.com>
Dear Team,

We have carried out CCTV inspection on new O2 piping (about 20m long of accessible opened flanged vertical and horizontal 6-in piping) installed during Revamp and visually found paintwork marks adjacent to wild joints, welding flux, stain mark which was a left-over mark by a CS metal plate laid inside the piping (inside the horizontal piping) and particulates. As per specifications the O2 piping shall be free from all contaminants which may react easily such as petroleum products (paintwork marks, oil, grease and organic materials) and shall be free from the presence of particulate matter which may react with O21 and/or eventually ignite the piping.

Seek your technical advice on the findings and greatly appreciate  to share on recommendations.
2




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...