Re: [MW:4337] RE: 4335] PWHT OF MATERIAL P No.5B

Dear Mr. R. Bathula,

Material  SA 335 Gr. P5
P No. 5B & Group No. 1

Thanks.
Manoj

On Thu, Feb 18, 2010 at 7:46 AM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:
Pl. indicate complete material specification (is it P5A, P5B and which group number?)


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of John Manoj
Sent: Wednesday, February 17, 2010 8:02 PM
To: materials-welding@googlegroups.com
Subject: [MW:4335] PWHT OF MATERIAL P No.5B
Dear all,

I need the following information. 

what is the soaking temperature?
what is the minimum holding time? 
What is the preheat and interpass temperature?

i have to make 1" sch 80 SA 335 Gr. P5  coil and there are 5 butt joints and i have to qualify wps aslo as per ASME SEC. IX.
As per ASME SEc. VIII Div. I normal holding temp. is 675 degree C and minimum holding time is 15 minutes. 
and as per ASME SEC. II part C Holding temp. is 745 degree C and holding time  is 1 hr./ in.

Thanks & Best Regards.

Manoj.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...