Dear All,

What I guess is the Question what Ali is asking was not understood properly by the group. He want confirmation that the Polarity will change the heat input or Not ?

Answer is in your Question Ali "heat input is independent from polarity" 

Now coming to your doubt on the statement you read somewhere where the percentage of Heat generated at Positive or negetive pole.... It is not only in GTAW but its applicable to all the Welding proces.

Please understand that the staement shows the distribution of total heat generated (100%) between the Electrdoe and Base Metal where the distribution of heat is always 70% on positve pole and 30% on negetive pole (again this % is approximate only). If you reverse the polarity % distribution between electrdoe and Base metal will interchange but total will remain 100%. .

Hope this suffice your doubt.

Regards.
C. K. Purohit
Eng-Tech Weld1
Sr Welding Inspector


On 12 February 2010 11:44, Ali Asghari <asghariali@rocketmail.com> wrote:
Hi All
all know that heat input is independent from polarity.but  i see in GTAW that in DCEN ,70%HEAT generated in arc concentrated in parent metal & in DCEP 30% HEAT concentrated in base metal.
can anybody clarify it?
regards.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...