[MW:4366] DSS REPAIR WELDING PROCEDURE

Hi everyone,
I need to inspect the castings of ASTM A 995 GR.4A(DSS). Now mfr. is having the approved/qualified wps for repair work. This material(castings) is having other requirements like ferrite content, pitting corrosion resistant test, sigma phase, total of intermetallic phases. The qualified wps doesn't consist these metallurgical tests, but having all mechanical and impact test. can mfr. go ahead with this wps for repair work? wps is having any relationship with these type of metallurgical tests?

With regards,
Rutvik

The INTERNET now has a personality. YOURS! See your Yahoo! Homepage. http://in.yahoo.com/

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...