[MW:4307] SSCC test for Welding in sour application.

We have carried out a SSCC test on the welding of API 5l Gr 60 pipe as per NACE TM 177 and ASTM G 36.
As per the lab test report which I have not physically verified out of 12 specimens one has failed.
As per the client spec requirement there shall be no cracks after 720 hrs. What is the normal acceptance criteria for this test as per code.I dont hav access to both the mentioned codes.
And also if a retest is allowed.Our major problem is already we hav welded using this WPS.

-

--
With Regards,
James

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...