Dear friends,
I need to run the new WPSin Aluminium steel plate using the attached grade of Aluminum plate.
How many times I have tried but I can not get the acceptable results from bend test.
It is broken after slight bending.
Can you help me please how to weld it to get the acceptable results from bending?
The wire I am using is ER5356 which is reccommended for this type of AL.
Best regards,