Hi!
Impact testing is a supllementary essential variable, Hence you need to run a pqr for P.No.1 Gr.2 material.
 
Regards,
vipin george

On Thu, Jan 7, 2010 at 8:33 PM, Chandra, Vasanthan (Lagos) <Vasanthan.Chandra@deltaafrik.com> wrote:

Friends,

 

I have come across a typical issue as below,

 

  1. Material is API 5L X-65 – S No 1 Gr.2
  2. Impact required at -29 deg.C
  3. Welding as per ASME Sec IX

 

I have a PQR which is SA 106 Gr B (P1 Gr 1) Impact tested at -30 deg.C

 

Can I support this PQR for S1 Gr 2 or P1 Gr 2? My client is rejected this and asking for PQR which was done on Group 2 materials either on S1 or P1.

 

Could you let me know, since my client is seeking evidence as per Sec IX? How to convince them that Gr 1 impact tested can also be used for Gr 2 materials.

 

 

 

Regards,

Vasanth

 


*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...