RE: [MW:3984] RE: 3979] Need confirmation as per code

Qualify the procedure with coupon in similar condition with all applicable variables including water temperature. Would be better to keep temperature of water colder than in actual condition.

(all subject to end user’s acceptamce)

Rgds

raj

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Nageswararao Nistala
Sent: Thursday, January 07, 2010 13:51
To: materials-welding@googlegroups.com
Subject: Re: [MW:3983] RE: 3979] Need confirmation as per code

 

Dear friends,

 

in my view no code permits for such practices but if client approves you can complete the hydrotest and dewater the line and complte the pad welding, After completion of the pad welding you can do the adiitional NDT on the Pad joints.

 

Regards

 

Nageswararao

On Thu, Jan 7, 2010 at 2:24 PM, Hamed <hamkan309090@gmail.com> wrote:

Hi

I never see in any standard or code to allow in this regard. So I think your Hydro test was rejected . you should release the water & weld the pad & again do the test.

 

Sincerely yours

Hamed Malekan

.Panahsaz Iran Eng. Co.

.Mechanical Expert (LPG Tanks in South Pars-Assaluyeh)

.Tel:  +98 21 88801179  - Fax: +98 21 88900756

 

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of nawab ali bhatti
Sent: Wednesday, January 06, 2010 2:42 PM
To: materials-welding@googlegroups.com
Subject: [MW:3979] Need confirmation as per code

 

 

Dear Members / Friends

 

I need code reference regarding following

                Q.1: Client wants to weld pads without releasing water?

                Q.2:  Can weld without releasing water, if yes what problems will appear  in          future?

                Q.3:  If we can weld, what is the code / standard acceptance criteria?   

                      subcontractor filled water for Hydrotest without completing the welding of some pads(plate 9mm) & shoe supports      

Materials as following

1.       Pipe Thickness is 23.83 mm

2.       Dia 18”

3.       Service : high pressure steam

4.       Design pressure/temperature is 53.4 bar/427C

5.       Test pressure is 148.2 Bar as per B31.3

 

 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...