Thursday, January 7, 2010

[MW:3990] WELDING CONSUMABLE FOR SMAW & SAW

Dear all,

I have to weld API 5L X70 to API 5L X70 butt joint.

Can you help me to select welding consumable for SMAW & SAW process.

I have selected 2 type of consumables i.e. Electrode E 9018G and Flux/Wire F9AO-EA2-A3 or  Electrode E8018C3 and Flux/wire F8A2 -  EA2-A2.

Which one is better? Is there any other proper electrode & flu/wire?

and i wanted to know whether PWHT is applicable if we weld with these electrodes.

This is first time i am using this material.

Your response is highly appreciated.

Thanks
Manoj John.