Sunday, January 3, 2010

Re: [MW:3948] Re: Usage of Y strainer joint

Dear Israr,
Thanks, But I am asking for y welded joint connection.
I shall attache the sketch along with this
please guide me.
Thanks and best regards,
k.Rajagopal
On Sun, Jan 3, 2010 at 2:26 PM, israr <ahmedisrar.nm@gmail.com> wrote:
Dear Mr. Rajagopal,

Pleas see Fig.328.5.4 C of ASME B31.3. which is acceptable, i think if
such branch connection is acceptable so u can use Y connection also.

Regards

Israr Ahmed
KSA
+966530417332



On Jan 2, 9:08 am, rajagopal kannan <rajagopal.kan...@gmail.com>
wrote:
> Dear members,
> Is "Y" type, branch connection is allowed as per ASME B 31.3?
> If not can you suggest any other construction code, which permits "Y" type
> connection.
> Thanks and Best Regards,
> K.Rajagopal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...