Hi ,
1. SS 410S is ER NiCr-3 for 1st and 2nd layer
2. SS 347 is ER 309Cb for 1st layer and ER 347 for 2nd layer.
I already instructed our contractor to qualified cladding procedure (GTAW process) based on ASME IX and API 582 but unfortunately our contractor refused to do it and claim their existing Cladding procedure SS 309L qualify to clad SS 410S and SS 347.
I don't know what to do now because I'm not well known about ASME IX. Please help and advice me. You cooperation is highly appreciated
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.