Hi,
Pre heating of weld joints is to remove the tensile residual stresses, due
to welding and to homogenise the material. Particularly tensile residual
stresses- If the tensile residual stress of the material exceeds more than
50 % of the yield stress of the material, it will lead to localised
yielding/cracking.
Regards,
Vaidehi ganesan,
Metallurgy and Materials Group,
IGCAR, Kalpakkam-603 102, India.
============================================================================
----- Original Message -----
From: "redbull" <mohanq8@gmail.com>
To: "Materials & Welding" <materials-welding@googlegroups.com>
Sent: Mon, Oct 26, 09 12:44
Subject: [MW:3544] Reason for preheating


>
> Dear friends,
>
> Is there any other reason for preheating of weld joints other than
> Code requirements (B31.3). any metallurgical requirement etc.,
>
> Regards,
>
> Mohan.
>
>

--------------------------------------------------------------------------------

No virus found in this incoming message.
Checked by AVG - www.avg.com
Version: 8.5.423 / Virus Database: 270.14.32/2459 - Release Date: 10/25/09
19:57:00


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...